Top Grade Kina Nickel-Plated Aluminum Strip Copper-Plated Aluminum Foil Tinned Aluminum Coil
ʻO kā mākou pahuhopu nui ka hāʻawi ʻana i kā mākou mea kūʻai aku i kahi pilina ʻoihana liʻiliʻi koʻikoʻi a kuleana, e hāʻawi ana i ka nānā pilikino iā lākou āpau no ka Top Grade.Kina nickel-plated Aluminum Strip Pepa Aluminum Paʻi keleaweTinned Aluminum Coil, Aloha mākou iā ʻoe e hui pū me mākou ma kēia ala o ka hoʻokumu ʻana i kahi ʻoihana holomua a maikaʻi.
ʻO kā mākou pahuhopu nui ka hāʻawi ʻana i kā mākou mea kūʻai aku i kahi pilina ʻoihana liʻiliʻi koʻikoʻi a kuleana, e hāʻawi ana i ka nānā pilikino iā lākou a pauKina nickel-plated Aluminum Strip, Pepa Aluminum Paʻi keleawe, Loaʻa iā mākou ma mua o 100 mau hana i loko o ka mea kanu, a he 15 pū kekahi hui hana e lawelawe i kā mākou mea kūʻai aku ma mua a ma hope o ke kūʻai ʻana. ʻO ka maikaʻi maikaʻi ke kumu nui no ka ʻoihana e kū i waho o nā mea hoʻokūkū ʻē aʻe. ʻO ka ʻike ʻana ʻo Believing, makemake ʻoe i ka ʻike hou aku? E hoʻāʻo wale i kāna mau huahana a me nā hoʻonā!
Hoʻolauna Huahana
Nickel metala he kiʻekiʻe paʻa i ka ea, ikaika passivation hiki, hiki ke hana i ka loa lahilahi passivation kiʻiʻoniʻoni i loko o ka lewa, hiki ke pale aku i ka corrosion o ka alkali a me nāʻakika, no laila, i ka huahana mea chemically paʻa i loko o ka hana a me ka alkaline kaiapuni,ʻaʻole maʻalahi e discolor, hiki. e oxidized wale nō ma luna o 600 ℃; ʻO ka papa nickel plating he paʻa ikaika, ʻaʻole maʻalahi e hāʻule; ʻO ka papa nickel plating hiki ke hana i ka ʻili o ka mea paʻakikī, hiki ke hoʻomaikaʻi i ke kūʻē ʻana o ka huahana a me ke kūpaʻa ʻana o ka ʻakika a me ka alkali, ke kūpaʻa ʻana o ka huahana, corrosion, maikaʻi ka hana pale ʻana. Ma muli o ka paʻakikī kiʻekiʻe o nā huahana nickel plated, maikaʻi loa nā kristal nickel plated, me ka polishability kiʻekiʻe, hiki i ka polishing ke hiki i ke aniani hiʻohiʻona, hiki ke mālama ʻia i ka lewa i ka wā lōʻihi, no laila hoʻohana mau ʻia no ka hoʻonani. ʻO ka nickel plated copper foil i hana ʻia e CIVEN METAL he maikaʻi loa ka hoʻopau ʻana o ka ʻili a me ke ʻano pālahalaha. Hoʻopili ʻia lākou a hiki ke laminated me nā mea ʻē aʻe. I ka manawa like, hiki iā mākou ke hana i kā mākou nickel-plated copper foil ma ka annealing a me ka ʻoki ʻana e like me nā koi o ka mea kūʻai aku.
Mea Kumu
● Kiʻekiʻe-pololei Rolled Copper Foil (JIS:C1100/ASTM:C11000) Cu maʻiʻo ma mua o 99.96%
Mānoanoa Mānoanoa kumu
● 0.012mm~0.15mm (0.00047 iniha~0.0059 iniha)
Laulā laula o nā mea kumu
● ≤600mm (≤23.62 iniha)
Kahua Mea Kumu
● E like me nā koi o ka mea kūʻai aku
Palapala noi
● Nā mea hana uila, nā uila, nā pila, nā kamaʻilio, nā lako a me nā ʻoihana ʻē aʻe;
Nā ʻāpana hana
Nā mea | Hiki ke hoohanaNikelaKa paʻi ʻana | Weld ʻoleNikelaKa paʻi ʻana |
Laulā laula | ≤600mm (≤23.62 iniha) | |
Mānoanoa | 0.012~0.15mm (0.00047 iniha~0.0059 iniha) | |
Mānoanoa Layer Nickel | ≥0.4µm | ≥0.2µm |
Nikela maʻiʻo o ka Nickel Layer | 80 ~ 90% (Hiki ke hoʻololi i ka ʻike nickel e like me ke kaʻina hana kuʻi ʻana o ka mea kūʻai aku) | 100% Nikela Maʻemaʻe |
Kūleʻa ʻili o ka Layer Nickel(Ω) | ≤0.1 | 0.05-0.07 |
Hoʻopili | 5B | |
Ikaika U'i | ʻO ka hoʻohaʻahaʻa haʻahaʻa haʻahaʻa ma hope o ke kau ʻana ≤10% | |
ʻO ka elongation | ʻO ka hoʻohaʻahaʻa haʻahaʻa haʻahaʻa ma hope o ke kau ʻana ≤6% |
ʻO kā mākou pahuhopu nui ka hāʻawi ʻana i kā mākou mea kūʻai aku i kahi pilina ʻoihana liʻiliʻi koʻikoʻi a kuleana, e hāʻawi ana i ka nānā pilikino iā lākou āpau no Top Grade China Nickel-Plated Aluminum Strip Copper-Plated Aluminum Foil Tinned Aluminum Coil, Aloha mākou iā ʻoe e hui pū me mākou i kēia. ala o ka hana ʻana i kahi ʻoihana holomua a maikaʻi pū.
Top Grade China Nickel-Plated Aluminum Strip, Copper-Plated Aluminum Foil, Loaʻa iā mākou i kēia manawa ma mua o 100 mau hana i loko o ka mea kanu, a he 15 pū kekahi poʻe hana e lawelawe i kā mākou mea kūʻai aku ma mua a ma hope o ke kūʻai ʻana. ʻO ka maikaʻi maikaʻi ke kumu nui no ka ʻoihana e kū i waho o nā mea hoʻokūkū ʻē aʻe. ʻO ka ʻike ʻana ʻo Believing, makemake ʻoe i ka ʻike hou aku? E hoʻāʻo wale i kāna mau huahana a me nā hoʻonā!